S-N Fatigue Curve Fitting (Basquin, ASTM E739)
S-N fatigue curve fitting regresses log fatigue life on log stress amplitude following ASTM E739, giving the Basquin curve, confidence band, design curve and endurance limit, with run-outs treated as right-censored lives.
S-N 피로 곡선 적합은 ASTM E739에 따라 로그 피로수명을 로그 응력 진폭에 회귀해 Basquin 곡선, 신뢰띠, 설계곡선, 피로한도를 구하며, 런아웃은 우측 중도절단 수명으로 다룹니다.
I tested specimens at several stress levels, some of which did not fail (run-outs); how do I fit the S-N curve and get a design curve?
여러 응력 수준에서 시편을 시험했고 일부는 파단되지 않았습니다(런아웃). S-N 곡선과 설계곡선은 어떻게 구하나요?
Following ASTM E739, regress log10 cycles to failure on log10 stress, because stress is the controlled variable, and use run-outs as right-censored observations in a maximum-likelihood fit. The fitted line gives the Basquin exponent and coefficient, and a one-sided tolerance bound for a low percentile at each stress gives the design curve.
When to use S-N Fatigue Curve Fitting (Basquin, ASTM E739)
- You have constant-amplitude fatigue test results at several stress or strain levels.
- Some specimens are run-outs that must be used as censored data instead of being discarded.
- You need a median S-N curve with confidence band, a design curve, or an endurance limit estimate.
When to use something else
- Only one stress level was tested; summarise the life distribution with a Weibull or lognormal fit instead.
- Loads were variable-amplitude; count cycles with rainflow counting and apply Miner damage.
Assumptions and requirements
- log10 life is normally distributed with constant variance across stress levels.
- The relation between log life and log stress (or log of stress minus the endurance limit) is linear.
- Specimens are independent and run-outs are right-censored at their stopped cycle count.
- The strain-life option needs the elastic modulus E and excludes run-outs; with run-outs, bands are Wald approximations.
What the analysis reports
- Coefficients A and B of log10 N = A + B log10 S with standard errors, Basquin b and fatigue strength coefficient
- Median curve with ASTM E739 confidence band and design curve at a chosen percentile and confidence
- Endurance limit (Stromeyer model) or strength at a reference life
- Lack-of-fit linearity F test when stress levels are replicated; strain-life coefficients for the Coffin-Manson-Basquin option
How to report it
The Basquin S-N curve fitted to [value] specimens ([value] run-outs) was log10 N = [value] - [value]·log10 S (s = [value]); the fatigue strength exponent was b = [value] and the [value]% / [value]% design life at S = [value] was [value] cycles.
Related methods
- Rainflow Cycle Counting and Miner Damage
- Accelerated Life Testing Analysis
- Life Distribution Identification
How this method is validated
이 방법의 검증 근거
- Independent computation. 2 reference tests compare the results with SciPy and lifelines.
독립 계산. SciPy·lifelines 대조 참조 시험 2건 통과.
Tolerances are relative differences (absolute differences for values near zero). R comparisons and reference tests are re-run before each release of the analysis engine.
허용오차는 상대 차이입니다(0 근처 값은 절대 차이). R 대조와 참조 시험은 분석 엔진을 배포할 때마다 다시 돌립니다.
Run S-N Fatigue Curve Fitting (Basquin, ASTM E739) on Quorant
- Data you need
- a table (CSV or Excel) with an outcome variable and predictor (feature) columns
- Price
- 400 credits for one analysis up to 10,000 rows (complexity level 3); larger or wider data costs more. Optional methodologist review: 1800 credits.
- Checking
- Compared with independent computations
- Before you pay
- A free pre-analysis diagnosis checks your data and gives an exact quote; nothing is deducted until you approve it.